  1. R

    Chips into a thin or a thick build?

    A question for those with some experience... is it better to broadcast chips in a thicker or a thinner epoxy coat? I have the choice of either putting down two 5 mil coats or a single 10 mil coat.
  2. R

    Bubbles in 1st (primer coat)

    Hi all. I'm using a 100% solids epoxy and was advised that I should apply 3 coats: The first works as a primer, add flakes to the 2nd coat and then anti-slip grit to the 3rd (clear). The floor was diamond ground, patched and well cleaned. Prep went well but after spreading the 1st coat I have...