    major problem with Muscle Gloss

    The floor was not damp, as we had no rain in weeks, the humidity was low, and floor dried for three days after prepping. No direction was given to mix either the resin or catalyst before mixing them together. Each kit contained the specific quantities to mix for application. No thinning was...
  2. J

    major problem with Muscle Gloss

    I have had a very bad experience with Muscle Gloss. I carefully followed the brief instructions printed on the containers. The Floor Prep worked well on the new concrete -7 weeks old so I have no complaint about adhesion. The epoxy was another story. My floor required 4 kits. After application...