Recent content by c20Dude

  1. C

    Bead Blasting Help

    Thanks
  2. C

    Bead Blasting Help

    Thanks. Any tricks to getting the as cast look again?
  3. C

    Bead Blasting Help

    I am bead blasting cast aluminum with #10 glass bead. The aluminum is bubbling and then pits form. I’m also getting squiggly lines in the metal. I’m running at 50psi and have dry air. What might be causing this. Anyway to fix it? I’m worried it may have ruined my piece.