    Urethane left milky/cloudy finish

    I think you're right about it being opaque where it was put down too thick. In the data sheet, it says 1 gallon will cover 358-537 sq ft. I have a 500 sq ft space so when I had a bit left at the end I re-covered some areas and that's where it's the worst. So, my question now is what is the...
  2. R

    Urethane left milky/cloudy finish

    I think you're right about it being opaque where it was put down too thick. In the data sheet, it says 1 gallon will cover 358-537 sq ft. I have a 500 sq ft space so when I had more left in the can near the end I started putting on a little heavier and that's where it's the worst. So, my...
  3. R

    Urethane left milky/cloudy finish

    I put down two coats of armorseal 1000 HS. Weather was good, overnight lows in the low 60s and humidity fine. I waited ~3 days after my second coat and put down my first coat of Rexthane and was planning to do my second coat this evening. The first coat went down clean and seemed to dry nice...
  4. R

    Garage Floor Temperatures

    I have read a lot of posts about the minimum temperatures to cure Epoxy but not able to find anything that shows for how long. I am using Armorseal HS and it has a minimum curing temperature of 50 degrees. Temperatures in Houston are hovering between a high of 65 during the days and high 40s...