I am restoring a Craftsman 65334 toolbox from 1973. I have stripped the paint and removed all of the rust through electrolysis. The second it comes out of the water it is immediately covered in rust again. I'm talking within seconds. Someone told me to soak it in phosphoric acid to remove the rust and that it would protect the metal box from getting rust on it again. I did this but the second I remove the phosphoric acid per the instructions for rust removal on the bottle it is completely covered in rust again. What the heck am I supposed to do to get a clean surface to prime? A lot of people say that I have to prime it immediately but there is no way to dry it off and prime it before the rust happens again. It literally takes seconds and its covered again. Any help would be greatly appreciated.