i just had my slab diamond honed and then treated with sr2 and xtreme hard densifier.
http://www.xtremepolishingsystems.com/Xtreme-Hard-Lythic-Densifier-Chemical-Hardener-p/xhd32oz.htm
http://www.xtremepolishingsystems.com/ameriposh-SR2-concrete-densifer-p/amp-sr2.htm
would putting on more of either make the surface harder or more sealed? or is it a once the chemical reaction happens theres no more that can be done sort of thing?
some history: my slab got caught in the rain just after floating it for 4 hours over a year ago, washing of the concrete cream layer, down to aggergate. we were able to power trowel some concrete back up, but the surface was very porous and soft. they ground down about a quarter inch, to much harder concrete with a lot of exposed aggregate. but there was still a small amount of weak and porous concrete left in patchy areas.
id love a quick answer before i move stuff back in... thanks!!
http://www.xtremepolishingsystems.com/Xtreme-Hard-Lythic-Densifier-Chemical-Hardener-p/xhd32oz.htm
http://www.xtremepolishingsystems.com/ameriposh-SR2-concrete-densifer-p/amp-sr2.htm
would putting on more of either make the surface harder or more sealed? or is it a once the chemical reaction happens theres no more that can be done sort of thing?
some history: my slab got caught in the rain just after floating it for 4 hours over a year ago, washing of the concrete cream layer, down to aggergate. we were able to power trowel some concrete back up, but the surface was very porous and soft. they ground down about a quarter inch, to much harder concrete with a lot of exposed aggregate. but there was still a small amount of weak and porous concrete left in patchy areas.
id love a quick answer before i move stuff back in... thanks!!