sluggerknuckles
Member
- Joined
- Jan 1, 2012
- Messages
- 8
So last nite at my first attempt at electrolysis, something went oddly wrong. I used cirtistrip to get all of the paint off of a mid 50s craftsman table saw. There was pitting so being **** about it I thought that I would try electrolysis to get the rust out of the pits and clean it up for the gold hammertone paint.
I started the electrolysis last nite around 1130 and went back to it at 930 this morning. It looks like the rust grew!!!! I now have rust where I did not have it before. where I had a small patch of pits I now have increased pitting.
Was it the metal? the mixture? not enough anodes or not enough power?
If someone can shoot me a message on how to post pics I can show you what happened. I am mad for sure because it was much cleaner with the hand stripping process.
BTW. I used around six gallons of water and a half of a cup of soda ash/arm and hammer detergent. Three rebars clamped to a rubbermaid bucket. Car battery charger (there are only two settings....10 amp and 2 amp so I picked 10 amp).
Thanks for all the input. I am so mad.......
I started the electrolysis last nite around 1130 and went back to it at 930 this morning. It looks like the rust grew!!!! I now have rust where I did not have it before. where I had a small patch of pits I now have increased pitting.
Was it the metal? the mixture? not enough anodes or not enough power?
If someone can shoot me a message on how to post pics I can show you what happened. I am mad for sure because it was much cleaner with the hand stripping process.
BTW. I used around six gallons of water and a half of a cup of soda ash/arm and hammer detergent. Three rebars clamped to a rubbermaid bucket. Car battery charger (there are only two settings....10 amp and 2 amp so I picked 10 amp).
Thanks for all the input. I am so mad.......