Getting ready to start my floor project on my 32x77 slab. Ups man pulled in tonight with 4 boxes no turning back now. Can't wait to put up some before and after shots. I have some questions maybe some of you can help me out.
How long after I acid wash should wait to apply product?

Any tips or pointers for the install plan on having me and three buddies maybe 2 cutting in 2 rolling or should I have more hands on deck for a slab that size?

Is there a good roller brand or nap length I should use and how do I know how thick to put it down each coat?

Lastly we are planning on having a wedding reception in the barn one week from Saturday does that give me enough time to do everything and have enough time for the epoxy to set up to handle tables and chairs. Thanks appreciate any advice and tip that anyone can offer.image.jpg
 
To avoid these ads, REGISTER NOW!

LegacyIndustrial

ALLIANCE MEMBER
Joined
Jun 7, 2010
Messages
7,995
Location
deerfield, IL
Mix one unit at a time, 3 minutes, low speed drill, large mix wand.
Pour into large paint trays, dip and roll.

3/8" nap roller, 18" is best for large areas.

Once the first coat is no longer tacky, start the 2nd, not allowing 24 hrs to pass between them.

Foor traffic can begin after 24 hours of cure.

Good luck!
 