I was just wondering if this has been isolated to hot humid climates. Up here in calgary it's usually really dry so I'm thinking it would give a great cohesion. That and the mishandled shipments seemed to be the 2 major issues.
My dad has tried the 2-part epoxy and was disappointed so I thought I'd give the urethane a try.
Also it doesn't say anything about using the flakes with no clearcoat, but I read it was not recommended. Can this be any worse the using a 2-part epoxy with the flakes scattered on top?
Thanks for any info.
My dad has tried the 2-part epoxy and was disappointed so I thought I'd give the urethane a try.
Also it doesn't say anything about using the flakes with no clearcoat, but I read it was not recommended. Can this be any worse the using a 2-part epoxy with the flakes scattered on top?
Thanks for any info.