Innovate1
Well-known member
Did a much needed sealing of the exposed agregate concrete pad outside the garage last weekend. Weather was about 60 so figured that was about ideal. Cool enough that it doesn't dry too fast. Used a long nap roller and used about the amount it said it would cover. Finished up several hours before sunset so plenty of time before it got cooler. We used Specshield WB that was recommended by the local commercial supply house. Next morning there was a slight white haze over big sections and a few spots that were totally white. I noticed a few drops on the top of the container that are white so the white spots are where there was excess material that didn't soak in. Anything I can do about this now? Not too worried about the slight haze but would like to fix the white spots. Is thinking they may go away with time wishful thinking?