R.Anderson
Well-known member
Did a search didn't see a thread on this so thought I take some pictures of some aluminum castings I'm getting ready for. Investment/lost foam casting is what I am doing here. Name plates, some blocks to machine into some plastic injection molds,and a small milling vise (no pictures of the last two yet).
I'm trying a premixed joint compound, I grabbed this box by mistake thinking it was the just add water type oops but I'm trying it anyways. With my other castings several years ago I used a texture compound or joint compound can't remember and it worked well.
I mixed in more water to some for the first few coats, makes it easier to get in the small detail niches. As it dried it formed cracks in the 90 degree corners. I just added some in and over the cracks that take care of it.
This is as far as I am now on this. I will be brushing on another coat or two. I plan on casting them during Christmas break.
I'm trying a premixed joint compound, I grabbed this box by mistake thinking it was the just add water type oops but I'm trying it anyways. With my other castings several years ago I used a texture compound or joint compound can't remember and it worked well.
I mixed in more water to some for the first few coats, makes it easier to get in the small detail niches. As it dried it formed cracks in the 90 degree corners. I just added some in and over the cracks that take care of it.
This is as far as I am now on this. I will be brushing on another coat or two. I plan on casting them during Christmas break.